Synthesis Of Metakaolin Using Ball Milling Machine Images

21 starting materials kaolin was supplied from general company for ceramic amp porcelain products sheeni egypt metakaolin mk was prepared by calcination of kaolin at 850 o c for 3 hours in a furnace with heating rate of 5 o cmin then milled in planetary ball mill for 30 min to produce mk powder having blaine specific surface area of 2120 m 2 kg and specific gravity of 2500 kgm 3.